May 13, 2022 #1 mohamed fayez Petroleum Joined Dec 31, 2021 Messages 1 Location AE what is meant by supply condition in iso 13847 clause 7.6.3.3 Supply condition shall i perform a separate wpqr for each type of fitting (flange , elbow , tee , weldolet)
what is meant by supply condition in iso 13847 clause 7.6.3.3 Supply condition shall i perform a separate wpqr for each type of fitting (flange , elbow , tee , weldolet)
May 13, 2022 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,942 Location GB Heat treated, cold worked, etc etc. The material condition rather than the product form. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote