Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Plasticity (stress(strain)) interpolation in Abaqus

Status
Not open for further replies.

skrat

Student
Joined
Nov 29, 2021
Messages
2
Location
SI
The stress-strain data for a plastic deformation is given in table. 

 I have two questions related to how that table is treated:
- How is data interpolated? Is it piecewise linear or something else?
- What if the plastic strain is larger than the maximum plastic strain provided in the table? I presume the data is extrapolated? But how? Using the linear interpolation between the last two points or something smarter?

Thank you

viber_image_2021-11-29_19-45-52-191_gvxiaf.png
 
In short, the interpolation is linear and outside of the specified range the values are held constant. These rules apply to most of the material definitions in Abaqus. For details check the documentation chapter "Material data definition".
 