Hi all,
Any idea how the anti-condensation coating on window glass works.
The layers, reflection of sun rays etc.
 
think about how condensation occurs - cool surface and warm moist air . . . not sure coatings will have any benefits.

think hydrophilic coatings.
 
I think this is a consequence of low-e coatings... taking the cooler surface 'outdoors'... When I installed low-e glazing in our home about 30 years ago... I noticed the condensation and thought nothing of it. With most glazing, you can stand adjacent to the window and 'feel the cold' from the outside... not with low-e.