Is it faisable to regrout a soil nail thats missing some grout days after it was grouted the first time.

Thank you
 
Yes, as long as the ungrouted drill hole has not collapsed. You have to fill up the hole some time. The sooner the better.
The bigger question is, "Why wasn't the hole fully grouted to begin with?"

 