CERAMIC ARMOUR
CERAMIC ARMOUR
(OP)
I am looking for specific information with reference to the manufacture, specification and performance of ceramic armour panels both personel and vehicle.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Contact USThanks. We have received your request and will respond promptly. Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting Guidelines |
|
Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.
Here's Why Members Love Eng-Tips Forums:
Register now while it's still free!
Already a member? Close this window and log in.
RE: CERAMIC ARMOUR
RE: CERAMIC ARMOUR
RE: CERAMIC ARMOUR
RE: CERAMIC ARMOUR
We are metallizing Titanium and ceramics, etc. with Titanium in them for use in brazing saws another tools. In this application we need a minimum of 50,000 psi. tensile. We start with an etching so that part is covered as well. It shouldn’t cost more than a half day of lab time ($500) to find out.
Tom
Mr. Thomas J. Walz
President
Northwest Research Institute, Inc. / Carbide Processors, Inc.
3847 S. Union Ave.
Tacoma, WA. USA 98409
800 346-8274
Ph (253) 476 1338
Fax (253) 476 1321
tomwalz@email.msn.com
www.carbideprocessors.com
RE: CERAMIC ARMOUR