Hi Everyone,

I remember that I have read somewhere that the most corrosive case in CO2-H2S environment is when the ratio of the partial pressures is 1.
Is this true? If yes, any reference please?

Regards,
Corroneer
 
Replies continue below

Recommended for you

I've never read that, and I've done a reasonable amount of reading on the subject.

Steve Jones
Corrosion Management Consultant


All answers are personal opinions only and are in no way connected with any employer.
 
In some environments there is a critical ratio (for carbon steel) but it depends on temp, pH, and a few other things.
I don't believe that this is a general condition.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy
 
@SJones and @EdStainless, thanks for the replies.
It seems that I am mistaken then!
 