Jan 7, 2020 #1 Abhishekmaitra Petroleum Joined Dec 5, 2019 Messages 1 Location IN Hi, can someone tell me the European standard for Carbon Steel, Alloy Steel, and Stainless Steel Nuts and Bolts for High Pressure or High Temperature Service?
Hi, can someone tell me the European standard for Carbon Steel, Alloy Steel, and Stainless Steel Nuts and Bolts for High Pressure or High Temperature Service?
Jan 9, 2020 #2 MGZmechanical Mechanical Joined Apr 4, 2010 Messages 108 Location ES Hi, - Carbon steel: ISO 898 - Stainless steel: ISO 3506 - EN 1515 (specially part 4 if you have to fulfill PED) Regards Upvote 0 Downvote
Hi, - Carbon steel: ISO 898 - Stainless steel: ISO 3506 - EN 1515 (specially part 4 if you have to fulfill PED) Regards
Jan 10, 2020 #3 rotw Mechanical Joined May 25, 2013 Messages 1,143 Location CA Maybe the DIN (Germany)? https://en.wikipedia.org/wiki/Steel_grades Upvote 0 Downvote