How to achieve hardness of EN24 upto 60
How to achieve hardness of EN24 upto 60
(OP)
Hi. I am a manufacturer of furnaces. I recently supplied an annealing furnace to a client. The operating temp of the furnace is 950 Deg C. Can anyone provide any information on the process to follow to achieve hardness of EN 24 components to 60 HRc? All help is appreciated. Thanks.





RE: How to achieve hardness of EN24 upto 60