Weldability of Hastelloy G-35
Weldability of Hastelloy G-35
(OP)
Fellows,
We are going to be welding some Hastelloy G-35 to make a ASME vessel. We work with C276, C22, B2/3 occasionally, no issues. Obviously this is another class of the alloy group, and quite niche.
Any concerns different from C276? Any recommended reading? Anyone in here have experience with it?
Thanks
We are going to be welding some Hastelloy G-35 to make a ASME vessel. We work with C276, C22, B2/3 occasionally, no issues. Obviously this is another class of the alloy group, and quite niche.
Any concerns different from C276? Any recommended reading? Anyone in here have experience with it?
Thanks





RE: Weldability of Hastelloy G-35
Matching filler metal ERNiCrMo-22
I would expect G-35 to present fabrication challenges very similar to C-276.
"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
RE: Weldability of Hastelloy G-35
Best regards - Al