Recommend a plasma cutter table

Status
Not open for further replies.

tharding247365

Mechanical
Joined
Dec 30, 2014
Messages
39
Location
US
Looking for a plasma cutter to cut 3mm aluminum panels. Looking for high resolution accurate cuts.

Anybody have recommendations on a plasma cutter table? Want to use one with a hypertherm cutter.

A fiber laser would probably more suitable for this but they're too expensive.
 
<<<< A fiber laser would probably more suitable for this but they're too expensive. >>>>
Depends on the size of your panels, the 3mm with shop air is at the max of this laser,
but the price and quality is affordable.


Larry
 