INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Top curb angle
3

Top curb angle

Top curb angle

(OP)
Why do we use top curb angle for roof to shell attachment. Why don't we directly weld the roof to the shell?

RE: Top curb angle

Normally because tanks are not swiss watches and some allowance for shape tolerances is needed. Also the Curb angle acts as a stiffener as well.

RE: Top curb angle

I think the main reason is to help round up the shell prior to placing the roof.

RE: Top curb angle

Dear rockeo,

Why do we use top curb angle for roof to shell attachment?

1. It helps to maintain the rigidity of the shell.

2. It provides a space where you weld the roof.

Why don't we directly weld the roof to the shell?

The top shell course is the thinnest (say 6 mm) while the roof could also be of the same thickness. Impossible to make a fillet weld with the roof plate resting on the shell all the while maintaining the desired leg length of the fillet (in this case 6 mm).

Regards.

DHURJATI SEN
Kolkata, India

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login


Resources

Low-Volume Rapid Injection Molding With 3D Printed Molds
Learn methods and guidelines for using stereolithography (SLA) 3D printed molds in the injection molding process to lower costs and lead time. Discover how this hybrid manufacturing process enables on-demand mold fabrication to quickly produce small batches of thermoplastic parts. Download Now
Design for Additive Manufacturing (DfAM)
Examine how the principles of DfAM upend many of the long-standing rules around manufacturability - allowing engineers and designers to place a part’s function at the center of their design considerations. Download Now
Taking Control of Engineering Documents
This ebook covers tips for creating and managing workflows, security best practices and protection of intellectual property, Cloud vs. on-premise software solutions, CAD file management, compliance, and more. Download Now