Min distance "A" between reinforcing plate and vertical weld joint
Min distance "A" between reinforcing plate and vertical weld joint
(OP)
Good day
I have a distance (A)125mm between periphery of reinforcing plate and vertical weld joint of tank.
In API 650 it shown as A=150mm (Fig. 5.6).
Can we reduce distance "A" to 125mm (with RT or PWHT)?
Dia. of nozzle 6"
WTH of tank 8mm
Water Storage tank.
Reinforcing plate type RTR
Thanks





RE: Min distance "A" between reinforcing plate and vertical weld joint
API does not have a rule that reduces "A" below 150 mm.
RE: Min distance "A" between reinforcing plate and vertical weld joint