INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

WRONG YIELD STRESS AT 50C ON VVD

WRONG YIELD STRESS AT 50C ON VVD

WRONG YIELD STRESS AT 50C ON VVD

(OP)
Hı ,
I have a question abouth vvd ( vissual vessel design ) program.
For exapmle when i choose AD2000 for design standart and T max :50C material P355GH . VVD calculating with 355 mpa yield stress .As you know acc to 10028 yield stres at 50C for P355 gh is 343 mpa not 355 !!!... why is it calculating like that ?
When i enter 51C it is fixing , yield stress is being 342.6 mpa but for 50C it is calculating with 355mpa ...
For this reason i m entering 51 C on vvd when i need a calc for max working at 50 C .
İs it a kind of bug of this program or is that any point that im missing ? ..

RE: WRONG YIELD STRESS AT 50C ON VVD

I do not know the mentionned program.
But AD2000-W1:2006 subclause 6.7: The values indicated in material specifications ...for 20°C are valid up to 50° C, the values indicated for 100°c are valid up to 120°C...

RE: WRONG YIELD STRESS AT 50C ON VVD

(OP)
Thank you so much for your great answer . I got one more abouth AD2000 :) AD2000 B0 9.2.1 says you have to add 1 mm corrrosion allowance if you are using carbon steel .. But İM not sure is that neccesary? For example im designing an lpg or air tank and will be painted just from outside ( no protection from inside) am i have to add 1 mm corrosion allowance to min . thickness ? sometimes our customers wants vessel with carbon steel with 0 mm corrosion allOwance ( no protection from inside ) is it imposible for AD2000?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close