INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Related Articles

Jobs

impact test welding procedure

impact test welding procedure

impact test welding procedure

(OP)
my understanding if i do have impact test procedure i can also used same procedure for without impact test requirement.
please advice.
regards
stan

RE: impact test welding procedure

Assuming you are following ASME B&PV Code, Section IX, you can qualify an existing WPS with no impact for impact by using the WPS to generate a weld coupon and conduct impact testing only.

RE: impact test welding procedure

Yes, impact tested procedure can be used on a joint which does not need impacts.

RE: impact test welding procedure

Typically yes, but I believe it is possible to pick up some combinations under QW-403.5 that would not otherwise be permitted by QW-424 for a non-impact tested application.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close