May 10, 2017 #1 dust123 Chemical Joined Jul 24, 2016 Messages 14 Location AT Hay, does sbd has or knows Standard for accelerated aging of decor paper? thx dust
May 26, 2017 #2 EdStainless Materials Joined May 20, 2004 Messages 16,367 Location Waukesha WI USA There are ASTM standards for measuring degradation from simulating environmental UV exposure for paints, rubbers, and plastics. They are ASTM D specs. = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, Plymouth Tube Upvote 0 Downvote