Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

IRON CARBON DIAGRAM

IRON CARBON DIAGRAM

IRON CARBON DIAGRAM

(OP)
Hai,


Pls share me our knowledge about iron carbon diagram and it's uses how to understand easily it?


REGARDS,

G.SRIRAM.

Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action

RE: IRON CARBON DIAGRAM

You can easily do this activity on your own using the Internet, and search for the iron carbon phase diagram.

RE: IRON CARBON DIAGRAM

Many fundamental metallurgical tests devote one of the first chapters to this discussion.
There are lots of good detailed studies of this subject.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube

RE: IRON CARBON DIAGRAM

Join ASM course to learn more.

"Even,if you are a minority of one, truth is the truth."

Mahatma Gandhi.

RE: IRON CARBON DIAGRAM

(OP)
Dear
Mr.Arunmrao can you explain about ASM?

REGARDS,

G.SRIRAM.

Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action

RE: IRON CARBON DIAGRAM

An interesting guy from another planet!

RE: IRON CARBON DIAGRAM

asminternational.org
And yes their $1,000 courses are worth the money.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube

RE: IRON CARBON DIAGRAM

(OP)
Mr. EdStainless,

Thanking you

REGARDS,

G.SRIRAM.

Dream,Dream,Dream Dream transforms in to thoughts.And thoughts result in action

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close