INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Moist Ammonia Air Stress Cracking Test UL125

Moist Ammonia Air Stress Cracking Test UL125

Moist Ammonia Air Stress Cracking Test UL125

(OP)
Hi,Im looking information about Moist Ammonia Air Stress Cracking Test, i need to realize this test but i need to fabricate the chamber to realizae the test.

Anybody knows if a can use acrylic to fabricate the chamber????, or if exit an ASTM standard about this chamber??

or if someone can tell a link, book or PDF where i can find information appreciate it.

Best regards.

RE: Moist Ammonia Air Stress Cracking Test UL125

"UL 8-2007 Water Based Agent Fire Extinguishers", which is one of the standards that comes up in a quick internet search that calls out a "10 day moist ammonia air stress cracking test", appears to require a glass test chamber. You can find it on google

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close