INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

QQ-S-763C

QQ-S-763C

QQ-S-763C

(OP)
what is the mechanical properties of 303 stainless steel listed under QQ-S-763C?
thanks.

RE: QQ-S-763C

To my best knowledge QQ-S-763 doesn't list 303 which is a free cutting version of 302. 303 is covered by ASTM A 581.

RE: QQ-S-763C

(OP)
303 was listed in qq-s-763 revision C and older. not in rev D and later. C is no longer available (free) at government site.

RE: QQ-S-763C

Yes you are correct. Here is a note I have found in QQ-S-763E.

6.4 Classes 303, 303Se, 416, 416Se, 430F and 430F Se under QQ-S-763C
should be purchased to ASTM A 484 and ASTM A 582 or ASTM A 555 and 581.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close