INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Drop test for ER 70S A1

Drop test for ER 70S A1

Drop test for ER 70S A1

(OP)
I need to do drop test for ER 70S A1. I need to know whether drop test is required for qualifying 20MnMoNi55(SA 508 Gr 3)+ SA350GRLF2/ SA 515 Gr 70 joint using ER 70S A1?
I want to know whether it will pass the test and at what temperature?. Does any one have hand on experience with these material combination.

RE: Drop test for ER 70S A1

What welding standard are you using and does it define the "drop test?"

Best regards - Al

RE: Drop test for ER 70S A1

Do you mean a drop weight tear test or a Charpy V-notch impact test? What temperature; What energy values?? Generally speaking, drop weight tear tests are not defined by most Engineering/Construction Codes because of their expense and they are performed on full thickness specimens.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close