INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Cold forging
5

Cold forging

Cold forging

(OP)
I am a Mech. Eng. and working in Cold forging related industry, As i am new to this field and learning about tool and Die design
i need specifically cold forging related literature or technical data how to design tools and dies .
Hope experienced Guys help me here
Thanks in advance

Simran Hunjan

RE: Cold forging

5
The best information on this subject will be available from ICFG (International Cold Forging Group). Look through their online library, especially for the following:
Doc 3/82 General Aspects of Tool Design and Tool Materials for Cold and Warm Forging
Doc 6/82 General Recommendations for Design, Manufacture and Operational Aspects of Cold Extrusion Tools for Steel
https://www.icfg.info/no_cache/virtual-laboratory/...

Read this article and look for some of the references:
Learning Cold Forming Technology — Another Engineer’s Perspective
http://www.bluetoad.com/publication/?i=196015&...

Here are some good downloads that are free:

Tooling solutions for challenges in cold forging
http://www.umformtechnik.net/binary_data/2425559_1...

http://www.strecon.com/Tools---Containers-700.aspx
http://www.strecon.com/Precision-Forging-726.aspx
http://www.strecon.com/2006---2010-793.aspx
http://www.strecon.com/2000---2005-794.aspx

Heading Hints - A Guide to Cold Forming Specialty Alloys
http://www.cartech.com/uploadedFiles/Products/Prod...

PREDICTION OF FATIGUE LIFE OF COLD FORGING TOOLS BY FE SIMULATION AND COMPARISON OF APPLICABILITY OF DIFFERENT DAMAGE MODELS
http://www.kau.se/sites/default/files/Dokument/sub...

Tooling solutions for cold and warm forging applications for automotive and other segments
http://www.istma.org/istma-world/ISTMA_Conferenceh...

Improvement of product accuracy and tool life at precise cold forming by suitable die prestressing
http://www.rmz-mg.com/letniki/rmz57/RMZ57_0465-047...

The main aspects of precision forging
http://www.acme.pwr.wroc.pl/repository/191/online....

http://www.simufact-americas.com/references/

http://www.qform3d.com/?go=publications

http://www.deform.com

www.c3m.si/colt/presentations/03%20Procedure.pps

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close