INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Rubber to rubber adhesive?

Rubber to rubber adhesive?

Rubber to rubber adhesive?

(OP)
Dear all,

I need an adhesive for EPDM to EPDM rubber.
Water application and no Silicon.

Any ideas?

Thanks,

Herc

RE: Rubber to rubber adhesive?

What kind of stretch do you expect the bond to undergo?  

A good bonding adhesive for EPDM is...EPDM.  Talk to a roofing supply house, there are room temp. curing EPDM liquids and membranes, though they may be too soft.  I've tried bonding nitrile and epdm with the 3M product and similar evaporative rubber cements, with limited success.

RE: Rubber to rubber adhesive?

Mint's found a hammer.  Good thing he is finding plenty of nails ;)

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close