INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Suitable steels for 20% H2S environment

Suitable steels for 20% H2S environment

Suitable steels for 20% H2S environment

(OP)
Does anyone have any knowledge on suitable steels for manufacturing equipment for use in a 20% H2S environment? Normally I would use AISI 4140 limited to 22RC but not at this elevated level of H2S.
Thanks and regards,
Paul

RE: Suitable steels for 20% H2S environment

SAE 4130 with 22 HRC is widely used for these conditions.

RE: Suitable steels for 20% H2S environment

SAE 4130 modified by the addition of Mo (up to 0.75%) is often used at 22 HRC for these conditions.  Mo confers additional corrosion resistance in both Cl- and H2S conditions.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login



News


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close