Oct 30, 2009 #1 t1t2t3 Petroleum Joined Oct 26, 2009 Messages 13 Location ES Has any one here information about the damage and consequences coming from the use of Hard Stamp (Weld # and Welder #) instead of Low Stress over ss pipe 304 and 316. I'll stimate your answer