I would like to know the creep crack growth properties of CrMoV. what is the best source that could give me this information?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Contact USThanks. We have received your request and will respond promptly. Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting Guidelines |
|
RE: CrMoV creep crack growth
Would suggest you read the chapters on crack initiation and growth in "Fracture & Fatigue Control in Structures" by Barsom & Rolfe; published by Prentice & Hall.
ISBN 0-13-329863-9 025.
RE: CrMoV creep crack growth
BS7910:1999 appendix U has constants for creep crack growth estimation for a number of materials including CrMoV.