INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

CLADDED AND LINED CRA PIPE

CLADDED AND LINED CRA PIPE

CLADDED AND LINED CRA PIPE

(OP)
Dear Experts,
Can any body suggest the manufacturing process for cladded and line CRA pipe. Because API 5LD which is a relevent spec. for cladded or lined CRA pipe does not specifiy the proces of manufacturing.

RE: CLADDED AND LINED CRA PIPE

(OP)
Thanks Steve,

Further to the query do you have any idea why most of operating industry in oil gas sector prefers only metallurgic ally bonded pipe and not mechanically bonded pipe.

Regards,

   

RE: CLADDED AND LINED CRA PIPE

5L is pipeline work with long distance transport after coating, rough handling and lots of bending and sagging.

**********************
"Pumping accounts for 20% of the world's energy used by electric motors and 25-50% of the total electrical energy usage in certain industrial facilities."-DOE statistic (Note: Make that 99% for pipeline companies) http://virtualpipeline.spaces.live.com/

RE: CLADDED AND LINED CRA PIPE

Because they are frightened of having something loose down the middle of their pipeline.  The principal fear is liner collapse.   

Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
 

RE: CLADDED AND LINED CRA PIPE

(OP)
Dear Steve,
Do you know of any history of failure in lined pipe i.e.liner collapse.
Thanks  

RE: CLADDED AND LINED CRA PIPE

Not in service.  I do know of collapses in individual pipes at the coating plant.  But just to put things in perspective, there is lined pipe on the seabed; BP have put it in and Santos Exeter-Mutineer put some in a couple of years back. As I type, Petroleum Development Oman are installing about 25 km of 14 and 16-inch 825 lined pipe onshore.

Steve Jones
Materials & Corrosion Engineer
http://www.linkedin.com/pub/8/83b/b04
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login


Resources

White Paper - Considerations for choosing a 3D printing technology
The adoption of 3D printing into major companies’ product development life cycles is a testament to the technology’s incredible benefits to consumers, designers, engineers and manufacturers. While traditional production methods have limitations in manufacturability, 3D printing provides unparalleled design freedom due to the additive method of building parts layer by layer. Download Now
White Paper - Are all 3D printed metals the same?
With so many different 3D printing metal systems and processes today, how can you know exactly what you’re getting? Today, there are several different methods for manufacturing 3D printed metal components with their own strengths and limits. Download Now

Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close