I was looking to see if there was a way to properly connect
aluminum gutter to existing galvanized steel downspouts
 
Replies continue below

Recommended for you

Al rivets would work.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
You don't want the aluminum in contact with the steel, if you want to save the steel.

How about a transition made from, say, PVC?



Mike Halloran