manufacturing process for chromium oxide powders
manufacturing process for chromium oxide powders
(OP)
kindly let me know the various methods for commercial production of chromium oxide powders
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Contact USThanks. We have received your request and will respond promptly. Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting Guidelines |
manufacturing process for chromium oxide powders
|
Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.
Here's Why Members Love Eng-Tips Forums:
Register now while it's still free!
Already a member? Close this window and log in.
RE: manufacturing process for chromium oxide powders
You can see the methods in the books of Inorganic Chemistry.
It's obtained by reduction with combustion of K2Cr2O7 +S
The potassium dichromate can be sustituted by sodium dichromate,more cheap,and the sulphur by organic matter: glucose or other carbohydrate.