Greetings,

I am looking for a white or off white opaque epoxy. It should be rigid or semi rigid. 3M420 works well but dries clear. 3M605 is a nice opaque off white but is too flexible.

Any tips on this would be appreciated.

Steve
 
You might want to give these people a call. They have Silver and Carbon filled so off white should be no problem.

Depending on the quantity you might look at adding a little TiO2 to a batch of the clear.

 
3M has a bulk 420 that is off-white.

Additionally, 3M has 460, 1386 & 1469 that are white/off-white.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks very much to you both - I will let you know how this works out.

Regards,
Steve
 
Akemi or West Marine are good sources for color filled epoxies.
 