Non Asbestos Gaskets on Chlorine??

Status
Not open for further replies.

Biggy

Mechanical
Feb 5, 2002
35
With the use of CAF Gakets on chlorine duty being prohibited in the UK from the end of ther year, I need to find an alternative material.

What Non-Asbestos joints are being used around the world (for use on Dry Liquid Chlorine and Dry Gaseous Chlorine)?

Many thanks in anticipation....

 
Replies continue below

Recommended for you

Garlock "Gylon 3510" for both services is approved by the Chlorine Institute, according to my info. Check with the Institute at Cl2.com.
 