INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Active brazing of CFC

Active brazing of CFC

Active brazing of CFC

(OP)
Hello,

I need to join CFC to metal. Does anybody know a brazing-alloy I can use?

Thanks for all your answers!

RE: Active brazing of CFC

CFC = carbon fiber composite, chloro-floro-carbon, ???

What specific materials are you trying to join?

RE: Active brazing of CFC

(OP)
Hello Gentlemen,

thanks you for your replys. I'm trying to join carbon fiber composites with metal...please excuse that I didn't write that clearly.

RE: Active brazing of CFC

(OP)
What may be important too, is that the CFC-part will be used in high temperatures (>1000°C)...

RE: Active brazing of CFC

So what matrix material do you plan to use in the composite?  tianium?  inconel? ceramic?  what metal are you joining to?  1000C is very hot!

RE: Active brazing of CFC

(OP)
the matrix material will be carbon, the metal will inconel...what I want to know, is which brazing alloys I can use to wet the C/C...

RE: Active brazing of CFC

Why do you want to have a liquid metal contact your composite?  Why not use a liquid polymeric adhesive?

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.

RE: Active brazing of CFC

(OP)
because of the high temperatures the compound will be used in...

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login


Resources

Low-Volume Rapid Injection Molding With 3D Printed Molds
Learn methods and guidelines for using stereolithography (SLA) 3D printed molds in the injection molding process to lower costs and lead time. Discover how this hybrid manufacturing process enables on-demand mold fabrication to quickly produce small batches of thermoplastic parts. Download Now
Design for Additive Manufacturing (DfAM)
Examine how the principles of DfAM upend many of the long-standing rules around manufacturability - allowing engineers and designers to place a part’s function at the center of their design considerations. Download Now
Taking Control of Engineering Documents
This ebook covers tips for creating and managing workflows, security best practices and protection of intellectual property, Cloud vs. on-premise software solutions, CAD file management, compliance, and more. Download Now