INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

North American comparable Steel spec to China specs

North American comparable Steel spec to China specs

North American comparable Steel spec to China specs

(OP)
Could somebody please let me know the North american Steel spec for the following china specs.....
NF300
NF300+CR
FCDFH,FC250+WELD EDGE,SS400+ WELD EDGE
FC250+CR
FCDFH+CR
SKD11N+CR
SKD11N+NW
SKD11N+TD

THESE SPECS ARE FOR NISSAN DIE SPEC'S THAT THEY REQUIRE US TO USE FOR BUILDING THEIR TOOLS. IT WOULD BE GREAT TO KNOW THE  COMPARABLE SPEC. EXAMPLE 4140!    

RE: North American comparable Steel spec to China specs

First things first...

1) What general type of steels are these? Tool steels? 1008/1010.. Drawing grades, HSLA, ....

2) Are these market specs or are they internal Nissan specs...

3) Are they china or japan? Seems that prints originating at Nissan would be Japan.

4) I've never seen automotive specify tooling materials, are you sure? If so then these likely all have american grades....

Heres some quick help:
I couldnt find NFxxx in my book at all.
FCDnnn is Ductile Cast Iron to JISG5502 -- IE: Japan spec.
FCnnn is Grey Cast Iron to JISG5501 -- IE: Japan spec.
SKD11 is D2 Tool Steel to JISG4404 -- IE: Japan spec.

Thats the best I can get you w/o more detail.

Nick
I love materials science!

RE: North American comparable Steel spec to China specs

(OP)

 Thanks for your response! They are general tool steels. We are currently quoting tooling for Fabco which in turn is for Nissan. You are right to say that they are Japan spec's. I wasn't sure at the time. When we quote Nissan, sends there material needs in which we are in turn suppose to use for their tools. Thanks for your response and it is truely appreciated. If you stuble accross any of the other spec's just let me know?
  

RE: North American comparable Steel spec to China specs

You might try getting info from MATWEB or Global engineering Documents.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources


Close Box

Join Eng-Tips® Today!

Join your peers on the Internet's largest technical engineering professional community.
It's easy to join and it's free.

Here's Why Members Love Eng-Tips Forums:

Register now while it's still free!

Already a member? Close this window and log in.

Join Us             Close