Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

CF3 fatigue properties data?

Status
Not open for further replies.

snellen

Materials
Joined
Jun 30, 2005
Messages
6
Location
US
I cannot find any data for low and high cycle fatigue properties about this cast stainless. Any suggestion?

Gerard
 
Well, there are many that can help you here more than I can, but have you tried looking up it's astm equivalent?

I have it as ASTM A743 if it's as cast, and ASTM A744 if it's solution quenched.

I'm sure there are a lot of people in the forum that may know the fatigue properties, I can't help any further though.

good luck
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top