INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Contact US

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Testing Procedures or Specifications on The Rip-Rap

Testing Procedures or Specifications on The Rip-Rap

Testing Procedures or Specifications on The Rip-Rap

(OP)
My question is: Are there any written testing methods, procedures or specificaitons for the rip rap and gabion materials.

Thank you in advance.

RE: Testing Procedures or Specifications on The Rip-Rap

quite a few, I would suggest you check out the corps of engineers - they have extensive written specs indicating testing requirements that you may want to consider for both riprap and gabions.  

The specs are online at

 http://www.usace.army.mil/pubtypes.html

RE: Testing Procedures or Specifications on The Rip-Rap

AASHTO and ASTM standards re testing would have some procedures as well. You are likely looking for freeze thaw testing on rip rap materials etc.

Regards

RE: Testing Procedures or Specifications on The Rip-Rap

From my own experience, when dealing with Gabion stone, the size requirements relate directly to the size of Gabion basket proposed. Apart from this, there are generic requirements fro strength, durability, rock type etc... that are recorded in lots of specifications, but its the grading which is often the key thing.
As for Rip-Rap, as well as looking at what the material needs to do, always check what materials are available locally. I was involved in a project , where no quarry within 200 miles could produce a material which would meet the Clients very exacting requirements, and this went on for a couple of years until the specification was changed.

RE: Testing Procedures or Specifications on The Rip-Rap

(OP)
Thank you all for your reply.

I am now using ASTM D5519-94 for the Riprap materials test.

RE: Testing Procedures or Specifications on The Rip-Rap

You may want to try the new ASTM 6711 for gabion stone fill specs. This ties in nicely with ASTM 975 which is for the specification of woven mesh gabions & mattresses.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members! Already a Member? Login


Resources

Low-Volume Rapid Injection Molding With 3D Printed Molds
Learn methods and guidelines for using stereolithography (SLA) 3D printed molds in the injection molding process to lower costs and lead time. Discover how this hybrid manufacturing process enables on-demand mold fabrication to quickly produce small batches of thermoplastic parts. Download Now
Design for Additive Manufacturing (DfAM)
Examine how the principles of DfAM upend many of the long-standing rules around manufacturability - allowing engineers and designers to place a part’s function at the center of their design considerations. Download Now
Taking Control of Engineering Documents
This ebook covers tips for creating and managing workflows, security best practices and protection of intellectual property, Cloud vs. on-premise software solutions, CAD file management, compliance, and more. Download Now