Does anybody know the material ZeCor (and all its forms like ZeCor-Z, ZeCor-310M(T) etc)? I would like to know what the corrosion resistance is in hot (200 dCelcius) sulfuric acid (93 - 98%). They say it has a good resistance, but in compare to what? 904L??

Thanks in advance.

Mark
 
Replies continue below

Recommended for you

This alloy is proprietary, owned by MECS.
By good resistance they mean better than any other available alloy.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 