Aug 27, 2005 #1 2ndchild Petroleum Joined Aug 20, 2005 Messages 31 Location US hi, The Yield strength of the ASME A106 Gr B is 240MPa (35ksi)at 120C (250F)??? regards
Aug 27, 2005 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US 31.5 Ksi at 250 deg F (ASME Section II, Part D, Table Y-1). Upvote 0 Downvote