Should the 12 1/2% pipe tolerance be taken into account when performing nozzle load calculations using WRC-107?

Thanks
 
Replies continue below

Recommended for you

Yes. In general the minimum thickness (i.e. taking into account any forming and/or mill tolerance and corrosion allowances) should be used for stress analysis calculations.
 