Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

WPS

Status
Not open for further replies.

glazetm

Industrial
Joined
Jul 17, 2012
Messages
30
Location
US
I Have a wps for P1-P1 Plate with a thickness range form .187"-8" that requires stress relief to ASME VIII. Can i uses this wps to weld .5" plate that does not require stress relief? Or do in need a seprate wps for this lower thickness that does not require stress relief?
 
You must requalify a WPS without (no) PWHT per QW-407.1 and QW-253, -254, -255, etc.
 
You need to requalify without PWHT as AWS D1.1 also.
Regards
Aakash Jha

 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top