Mar 28, 2013 #1 kpm21443 Industrial Joined Dec 20, 2012 Messages 56 Location KW What is the meaning of the below statement. How should the UFD be done. Witness UFD (Ultrasonic Flaw Detection)of weld overlayed valve to check for dis-bonding.
What is the meaning of the below statement. How should the UFD be done. Witness UFD (Ultrasonic Flaw Detection)of weld overlayed valve to check for dis-bonding.
Mar 28, 2013 1 #2 hsbcn Mechanical Joined May 15, 2009 Messages 254 Location ES UFD is an NDE that checks for cracks and fissures by propagating sound waves through solid material. The NDE is carried out using a quite simple electronic device. High-alloy valves for corrosive petrochemical applications. Upvote 0 Downvote
UFD is an NDE that checks for cracks and fissures by propagating sound waves through solid material. The NDE is carried out using a quite simple electronic device. High-alloy valves for corrosive petrochemical applications.