Does anyone have the A*E properties and weight for 7-19 wire rope or the area, weight and the E values for same? I'm looking for 1/2" dia to 1" dia for an Smath program

Thanks, Dik

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Check out this engineering guide by US Steel. It's an older manual, but there is a wealth of information in it.

They even have sample calculations and the statics of common setups.

 
 https://files.engineering.com/getfile.aspx?folder=348c4667-c5ec-466e-89fb-2751407bf0c1&file=USS_Wire_Rope_Engr_HandBook.pdf
Thanks Gentlemen (Binary)... Contractor want to use wire rope for temporary guardrail...

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
You may find some relevant design information in the NCHRP report 711 from FHWA.

Rod Smith, P.E., The artist formerly known as HotRod10
 
Thanks, Bridge...

PEinc... Wire rope, not prestressing cable... I think the contractor is opting for a 'tie-off' cable, not a 'cable guard'...

Joel... your reference has good information about the equivalent Young's modulus for different wire rope types...

again... thanks.

-----*****-----
So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates

-Dik
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top