Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

WIRE MESH FOR CONCRETE WORKS 1

Status
Not open for further replies.

Erasa

Civil/Environmental
Jan 3, 2016
44
Hello
I need some clarification on this;
In AC 150/5340-30G; Figure 126(FAA), Standard Details for Taxiway Hold and Guidance Sign (Page 254).
What does the Wire Mesh 6” x 6”[15cm x 15cm] No.6 means? I know the 6” x 6” is the spacing of the wires but what I need to understand is the No.6.

Erasa
 
Replies continue below

Recommended for you

I don't have a copy of the document you reference, but the following is the typical definition of the WWR style/nomenclature:

Capturebbbb_f4ys91.png


CaptureAAA_rfs1u9.png


So for your case "6x6-W6xW6" would be plain (undeformed) wires at 6" long't and trans spacing, with each wire of cross sectional area of 0.060 in2
 
The "6" is the gauge (size) of the wire. It is usually the same in both directions but can be different as noted by Ingenuity

 