Also are there any other alloys that exhibit the same properties.
 
You can view many binary alloy (and a few ternary) phase diagrams at Solder alloys typically involve 2 or more of the following: Ag, Bi, Cu, In, Pb, Sn.
Present researches on solder alloys are directed toward 1) replacement of toxic Pb and 2) increased reliability (resistance toward thermal fatigue and the growth of Sn whiskers, etc.). A portion each June issue of JOM is devoted to lead-free solders, e.g.,
You can view the abstracts for free (entire articles if you are a TMS member).

A Pb-Sn phase diagram is below:

Pb_Sn.GIF



A liquidus surface of the Ag-Cu-Sn system used in some lead-free alloys is below:

sn_cu_ag.gif
 