Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Which Steel Stress for Crack Width Calculation for Multi-Layer Reinforcement?

Status
Not open for further replies.

bdbd

Geotechnical
Joined
Sep 17, 2015
Messages
144
Location
DK
Hi!
Very short but hard question: When you have more than one layer of reinfoircement on tension face, which steel stress should be used for crack width calculation and can you provide a reference to your answer?
A) Outermost reinforcement's stress
B) Stress at the centroid of the tensile reinforcement
 
I would suppose it would depend on what you're using for the thickness of the concrete cover. I would use the concrete cover to the outermost layer, and so I'd use tension stress in the outermost layer of reinforcing. It seems to me the crack width is related to the strain in the reinforcing and the distance to the face of the concrete, so additional layers of reinforcing are irrelevant to the crack width.
 
I agree with BridgeSmith.

Since strain and stress are assumed to linear, I suspect that using the centroid values, which would reduce the stress but increase the cover, wouldn't make much difference, but I haven't checked.


Doug Jenkins
Interactive Design Services
 
I suspect that using the centroid values, which would reduce the stress but increase the cover, wouldn't make much difference, but I haven't checked.

because the decrease in stress is minimal, but the increase in cover is substantial, it makes the required reinforcement spacing quite a bit smaller.
 
Status