Hello, from the standpoint of efficiency, you should consider that as a function of pH hypochlorite is effective at pH 6 -7. What I see is that you can have long-term scaling problems due to the form of calcium. If you can use sodium hypochlorite would be excellent.
Greetings.
Manuel Arguelles