Jun 25, 2003 #1 joecontrol Industrial Joined Sep 17, 2002 Messages 66 Location US Any information on the process of electro galvanizing wire. I currently work in the hdg industry and would like to get informed about this process.
Any information on the process of electro galvanizing wire. I currently work in the hdg industry and would like to get informed about this process.
Jul 24, 2003 #2 JimMetalsCeramics Materials Joined Jul 8, 2003 Messages 295 Location US I think you are looking for zinc electroplating. You should look for local plating shops and ask them if they plate zinc. Other options include brush plating (e. g., http://www.brushplate.com) and zinc paints (e. g., http://www.zingacoating.com). Upvote 0 Downvote
I think you are looking for zinc electroplating. You should look for local plating shops and ask them if they plate zinc. Other options include brush plating (e. g., http://www.brushplate.com) and zinc paints (e. g., http://www.zingacoating.com).