Hey,

I made a model of a wheel consisting of three different concentric layers, aluminium-rubber-aluminium. Then I have the wheel rotate and in the same time a track approaches the wheel. The wheel is supposed to just ride over the track, but it blows up & deforms (second picture) and even goes through the track.
Does someone know what is going wrong?
 
 https://files.engineering.com/getfile.aspx?folder=e21d99fb-39a8-4d68-831c-4f84282d6133&file=forum2in1.JPG
Did you define contact in this analysis ? You can use general contact capability. It works best. What are the boundary conditions and how are they applied (it would be best to show them on the picture) ?
 
Is the deformation scale factor larger than 1 in postprocessing?
Otherwise check if NLGEOM is on.
If that does not solve the problem, run the analysis in double precision.
 