Hi, does anyone know SS 316's compatibility with 316?



Please do drop more information or knowledge you have on this subject they will all be taken in and appreciated.


David O.
Mechanical Engineer
Graduate as of: 2007
Oil, Gas & Power
 
Corrosion? Welding? Other?

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Welding & Corrosion & Others (that you know)

Please do drop more information or knowledge you have on this subject they will all be taken in and appreciated.


David O.
Mechanical Engineer
Graduate as of: 2007
Oil, Gas & Power
 
Welding: compatible with each other; typically use E308 filler metal

Corrosion: compatible, 304 has lower resistance to Cl-

Other: they usually have terrible compatibility for threaded connections, especially with cut threads

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Why did you raise such a doubt. Most often they pose no major problem in conjunction,though 304 has lower corrosion resistance. If you are more specific,you will get a more meaningful response. Else, it appears more like an assignment.

I have not failed. I've just found 10,000 ways that won't work." — Thomas Edison
_____________________________________
 
Thanks for the responses guys, appreciate it and awaitin more if possible

Please do drop more information or knowledge you have on this subject they will all be taken in and appreciated.


David O.
Mechanical Engineer
Graduate as of: 2007
Oil, Gas & Power
 
Hi daviwy! 304 is considered "more machinable" than 316 due to its lower chrome composition. This is what makes 304 less corrosive resistant than the 316. There is a 316L grade available that will machine very well and provide excellent corrosive resistance. 316 is usually used in wet enviros and/or corrosive enviros. Cost of the 316 is about 20 percent more. welding 316: the welds must be passivated to ensure integrity of corrosive resistance at the surface. If you could supply info on the end use of the product I may recommend a grade to meet your needs.

Hope this helps!

Dingus
 
Totally agree with Dingus it is much easier to handle cut and bend most people opt for 304 for that reason.

Type 316—the second most common grade (after 304 for food and surgical stainless steel uses alloy addition of molybdenum prevents specific forms of corrosion. It is also known as marine grade stainless steel due to its increased resistance to chloride corrosion compared to type 304. 316 is often used for building nuclear reprocessing plants. 316L is an extra low carbon grade of 316, generally used in stainless steel watches and marine applications due to its high resistance to corrosion.

Hevs
Conveyor Manufacturers
 
For welding 316 to itself, I would use 316 or 316L filler metal for optimum corrosion resistance.
 