Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

What is "valve rating" and "Valve class" ?what differencre

Status
Not open for further replies.

osuamp

Mechanical
Jul 3, 2003
8
What is "valve rating" and "Valve class" ?what differencre?
 
Replies continue below

Recommended for you

Valve rating is nothing but the maximum pressure a valve can withstand or a pressure which valve designed.

Class are meant for Flange design.
 
The rating of a valve if you take B16-34 is the maxiumum pressure (psig) at a specified temperature (deg F) for a specified material (ASTM/ASME).

A Class covers all the ratings for the particular material within the specified temperature range.

For example Class 150 for WCB would cover all the pressure ratings from -20F to 1000F for that material. (It also covers both standard and special class)

Hope this helps.
 