Dear all
the reading on ASME SEC.II SA-20 2019ED
8.3.2.1 A total aluminum content of 0.020 % or more.
8.3.2.2 An acid soluble aluminum content of 0.015 % or more.
8.3.2.3 ....
8.3.2.4 ....
8.3.2.5 The analysis for the elements mentioned in 8.3.2.1, 8.3.2.2, 8.3.2.3, or 8.3.2.4 shall be included in the test report.
I got a SA-516-70 certificate and only had aluminum content 0.048% listed in it.
Can it correspond to 8.3.2.5 requirement?
the reading on ASME SEC.II SA-20 2019ED
8.3.2.1 A total aluminum content of 0.020 % or more.
8.3.2.2 An acid soluble aluminum content of 0.015 % or more.
8.3.2.3 ....
8.3.2.4 ....
8.3.2.5 The analysis for the elements mentioned in 8.3.2.1, 8.3.2.2, 8.3.2.3, or 8.3.2.4 shall be included in the test report.
I got a SA-516-70 certificate and only had aluminum content 0.048% listed in it.
Can it correspond to 8.3.2.5 requirement?