gmill

Materials
Aug 24, 2007
1
I need to know what type of material MS-6000 (D) 44A is.

 
Replies continue below

Recommended for you

MS-6000<D> is a Chrysler standard entitled ZINC AND ZINC-IRON ALLOY COATED SHEET STEEL. The 44A indicates a zinc-iron alloy coating with a specific coating weight (mass). There should be an additional designation for the grade that would like something like this:

MS-6000<D> 44A -050XF

The 050XF indicates a high-strength low alloy steel grade. You need to obtain the standard to understand all of the requirements. You will need to contact Chrysler directly in order to obtain this standard.
 