Apr 18, 2002 #1 THEHERR Materials Joined Mar 1, 2002 Messages 4 Location US RECENTLY, WE HAD A POTENTIAL CUSTOMER MENTION THIS STANDARD IN AN INQUIRY. DOES ANYONE KNOW WHAT THIS STANDARD COMPRISES AND WHERE I CAN GET A COPY? JOHN HERR APPLIED BOLTING HERR@APPLIEDBOLTING.COM
RECENTLY, WE HAD A POTENTIAL CUSTOMER MENTION THIS STANDARD IN AN INQUIRY. DOES ANYONE KNOW WHAT THIS STANDARD COMPRISES AND WHERE I CAN GET A COPY? JOHN HERR APPLIED BOLTING HERR@APPLIEDBOLTING.COM
Apr 18, 2002 2 #2 Hush Mechanical Joined Dec 21, 2001 Messages 317 Location US EN 10204 (formerly DIN 500049) details documentation requirements for material test certificates. Available from the British Standards Institution (BSI) or German (DIN). Upvote 0 Downvote
EN 10204 (formerly DIN 500049) details documentation requirements for material test certificates. Available from the British Standards Institution (BSI) or German (DIN).
May 27, 2003 1 #3 snowy2003 Mechanical Joined May 27, 2003 Messages 1 Location CA ISO 10204 is also the same available from the ISO Book store for a mear 65$ Upvote 0 Downvote